General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.75 g/cm³ Show Supplier Material materials with Density of 1.75 g/cm³ | ISO 1183 |
Water absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Water absorption of 0.01 % | SABIC method | 23°C/24hrs |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 0.6 % Show Supplier Material materials with Elongation of 0.6 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 13.5 GPa Show Supplier Material materials with Flexural modulus of 13.5 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 73 MPa Show Supplier Material materials with Flexural strength of 73 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 3 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 24 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 24 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 7 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 70 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 70 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 53 MPa Show Supplier Material materials with Tensile strength of 53 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 165°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | ISO 11359-2 | -30°C to 80°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 2.39E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 2.39E-5 1/K | ISO 11359-2 | -30°C to 80°C | ||
Heat deflection temperature | 231 - 275 °C Show Supplier Material materials with Heat deflection temperature of 231 - 275 °C | ||||
Heat deflection temperature, 0.45 MPa | 275 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 275 °C | ASTM D 648 | 3.2 mm | |||
Heat deflection temperature, 1.80 MPa | 231 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 231 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 18 W/(m·K) Show Supplier Material materials with Thermal conductivity of 18 W/(m·K) | ISO 22007-2 | 60*60*3mm plaque | ||
Thermal conductivity, through-plane | 23.0 °C | 1.3 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 1.3 W/(m·K) | ISO 22007-2 | 60*60*3mm plaque | ||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344589- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.2mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100960980- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Hot-Wire Ignition | 23.0 °C | 1.2 mm Show Supplier Material materials with Hot-Wire Ignition of 1.2 mm | ≥, UL 746A | PLC 0 |
Sheet resistivity, ROA | 23.0 °C | 25000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 25000 Ω | >, ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wiring Devices, LED Lighting, Electronic Components, Enclosure/Housing/Cover | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |