General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | ISO 1183 |
Water absorption | 23.0 °C | 0.5 % Show Supplier Material materials with Water absorption of 0.5 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 0.3 GPa Show Supplier Material materials with Elastic modulus of 0.3 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 90 % Show Supplier Material materials with Elongation of 90 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 0.3 GPa Show Supplier Material materials with Flexural modulus of 0.3 GPa | ISO 178 |
Flexural strength | 23.0 °C | 12 MPa Show Supplier Material materials with Flexural strength of 12 MPa | ISO 178 |
Hardness, Shore D | 23.0 °C | 56 [-] Show Supplier Material materials with Hardness, Shore D of 56 [-] | ASTM D 2240 |
Impact strength, Izod notched | 23.0 °C | 150 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 150 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 23 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 23 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 580 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 580 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 22 MPa Show Supplier Material materials with Tensile strength of 22 MPa | ASTM D 638 | break |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.1E-4 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 1.8E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.8E-4 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 57 - 88 °C Show Supplier Material materials with Heat deflection temperature of 57 - 88 °C | ||||
Heat deflection temperature, 0.45 MPa | 88 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 88 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 57 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 57 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093722- - <br> UL Recognized, 94HB Flame Class Rating: 1mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Document Handling, Lawn/Garden | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |