General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 2.07 g/cm³ Show Supplier Material materials with Density of 2.07 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.4 GPa Show Supplier Material materials with Elastic modulus of 3.4 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4.4 % Show Supplier Material materials with Elongation of 4.4 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 4.6 GPa Show Supplier Material materials with Flexural modulus of 4.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 105 MPa Show Supplier Material materials with Flexural strength of 105 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 17 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 55 MPa Show Supplier Material materials with Tensile strength of 55 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 130 - 140 °C Show Supplier Material materials with Heat deflection temperature of 130 - 140 °C | |
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 130 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 130 °C | ASTM D 648 | 3.2mm, unannealed |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 100MHz | 23.0 °C | 6.58 [-] Show Supplier Material materials with Dielectric constant, 100MHz of 6.58 [-] | IEC 60250 | 100 MHz |
Dielectric constant, 1GHz | 23.0 °C | 6.16 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 6.16 [-] | IEC 60250 |
Dielectric constant, 500MHz | 23.0 °C | 6.47 [-] Show Supplier Material materials with Dielectric constant, 500MHz of 6.47 [-] | IEC 60250 |
Dissipation factor, 100MHz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 100MHz of 1E-3 [-] | IEC 60250 | 100 MHz |
Dissipation factor, 1GHz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 1E-3 [-] | IEC 60250 |
Dissipation factor, 500MHz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 500MHz of 1E-3 [-] | IEC 60250 |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |