Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4.3 GPa Show Supplier Material materials with Elastic modulus of 4.3 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural strength | 23.0 °C | 172 MPa Show Supplier Material materials with Flexural strength of 172 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Tensile strength | 23.0 °C | 92 MPa Show Supplier Material materials with Tensile strength of 92 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | ||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥0.41mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221097- - <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Technological properties
Property | ||
---|---|---|
Application areas | Respiratory, Monitoring and Imaging, Air Cabin Interiors, Electronic Components, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 340 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |