General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.27 - 0.36 [-] Show Supplier Material materials with Coefficient of friction of 0.27 - 0.36 [-] | ||
Coefficient of friction, kinetic | 0.36 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.36 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.27 [-] Show Supplier Material materials with Coefficient of friction, static of 0.27 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.41 g/cm³ Show Supplier Material materials with Density of 1.41 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 20.1 GPa Show Supplier Material materials with Elastic modulus of 20.1 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 1.2 % Show Supplier Material materials with Elongation of 1.2 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 22.7 GPa Show Supplier Material materials with Flexural modulus of 22.7 GPa | ISO 178 |
Flexural strength | 23.0 °C | 334 MPa Show Supplier Material materials with Flexural strength of 334 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 8 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 96 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 96 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 39 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 39 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 939 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 939 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 214 MPa Show Supplier Material materials with Tensile strength of 214 MPa | ISO 527 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 279 °C Show Supplier Material materials with Heat deflection temperature of 279 °C | ||
Heat deflection temperature, 1.80 MPa | 279 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 279 °C | ASTM D 648 | 3.2mm, unannealed | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101345286- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101345253- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Lab Ware and Clinical Diagnostics, Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |