General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.21 - 0.25 [-] Show Supplier Material materials with Coefficient of friction of 0.21 - 0.25 [-] | ||
Coefficient of friction, kinetic | 0.25 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.25 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.21 [-] Show Supplier Material materials with Coefficient of friction, static of 0.21 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.16 g/cm³ Show Supplier Material materials with Density of 1.16 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.42 % Show Supplier Material materials with Moisture absorption of 0.42 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4.3 GPa Show Supplier Material materials with Elastic modulus of 4.3 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 3.3 % Show Supplier Material materials with Elongation of 3.3 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 3.7 GPa Show Supplier Material materials with Flexural modulus of 3.7 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 131 MPa Show Supplier Material materials with Flexural strength of 131 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 32 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 603 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 603 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 86 MPa Show Supplier Material materials with Tensile strength of 86 MPa | ASTM D 638 | break |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.5E-5 1/K | ASTM E 831 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 5.93E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.93E-5 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature | 118 - 253 °C Show Supplier Material materials with Heat deflection temperature of 118 - 253 °C | ||
Heat deflection temperature, 0.45 MPa | 253 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 253 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 118 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 118 °C | ASTM D 648 | 3.2mm, unannealed | |
Thermal conductivity | 23.0 °C | 0.29 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.29 W/(m·K) | ASTM E 1530 | |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Industrial Material Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |