General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.22 [-] Show Supplier Material materials with Relative density of 1.22 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 110 % Show Supplier Material materials with Elongation of 110 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.7 GPa Show Supplier Material materials with Flexural modulus of 2.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 95 MPa Show Supplier Material materials with Flexural strength of 95 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 133 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 133 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 133 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 133 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 51 MPa Show Supplier Material materials with Tensile strength of 51 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 82 °C Show Supplier Material materials with Heat deflection temperature of 82 °C | ||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100900880- - <br> UL Recognized, 94-5VB Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 1 V Show Supplier Material materials with Comparative tracking index of 1 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Pharmaceutical Packaging & Drug Delivery, Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 75 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |