General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 15 % Show Supplier Material materials with Elongation of 15 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 69 MPa Show Supplier Material materials with Flexural strength of 69 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 101 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 101 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 101 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 101 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 587 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 587 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 39 MPa Show Supplier Material materials with Tensile strength of 39 MPa | ASTM D 638 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 80 °C Show Supplier Material materials with Heat deflection temperature of 80 °C | ||
Heat deflection temperature, 1.80 MPa | 80 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101345218- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |