General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.17 [-] Show Supplier Material materials with Coefficient of friction of 0.17 [-] | ||
Coefficient of friction, kinetic | 0.17 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.17 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Density of 1.31 g/cm³ | ASTM D 792 |
Water absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Water absorption of 0.05 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Elastic modulus of 2.1 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 5.5 % Show Supplier Material materials with Elongation of 5.5 % | ISO 527 | yield |
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ISO 178 |
Flexural strength | 23.0 °C | 82 MPa Show Supplier Material materials with Flexural strength of 82 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 19 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 19 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 302 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 302 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 129 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 129 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2000 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2000 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 23 J Show Supplier Material materials with Instrumented Impact, at Peak of 23 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | ISO 527 | yield |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 127 °C Show Supplier Material materials with Heat deflection temperature of 127 °C | ||
Heat deflection temperature, 1.80 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 127 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101343864- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.7mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 18.1 g/10min Show Supplier Material materials with Melt mass-flow rate of 18.1 g/10min | ASTM D 1238 | 300°C/2.16 kgf | |
Shrinkage | 23.0 °C | 0.68 % Show Supplier Material materials with Shrinkage of 0.68 % | SABIC method | 1.5-3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.67 % Show Supplier Material materials with Shrinkage, transverse of 0.67 % | SABIC method | 1.5-3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |