General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.32 [-] Show Supplier Material materials with Relative density of 1.32 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 33.3 GPa Show Supplier Material materials with Elastic modulus of 33.3 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 252 % Show Supplier Material materials with Elongation of 252 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 25 GPa Show Supplier Material materials with Flexural modulus of 25 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 390 MPa Show Supplier Material materials with Flexural strength of 390 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 8 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 116 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 116 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1069 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1069 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 259 MPa Show Supplier Material materials with Tensile strength of 259 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 255 °C Show Supplier Material materials with Heat deflection temperature of 255 °C | ||
Heat deflection temperature, 1.80 MPa | 255 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 255 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282584- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 10000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Electronic Components, Audio | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |