General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Density of 1.37 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.83 % Show Supplier Material materials with Moisture absorption of 0.83 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.35 [-] Show Supplier Material materials with Relative density of 1.35 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 9.7 GPa Show Supplier Material materials with Elastic modulus of 9.7 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 8.1 % Show Supplier Material materials with Elongation of 8.1 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 6.8 GPa Show Supplier Material materials with Flexural modulus of 6.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 157 MPa Show Supplier Material materials with Flexural strength of 157 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 53 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 53 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 727 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 727 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 16 J Show Supplier Material materials with Instrumented Impact, at Peak of 16 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 35 MPa Show Supplier Material materials with Tensile strength of 35 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 135 - 141 °C Show Supplier Material materials with Heat deflection temperature of 135 - 141 °C | ||
Heat deflection temperature, 0.45 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 141 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 70 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 70 °C | UL 746B | |
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093413- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |