General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 7.9 GPa Show Supplier Material materials with Elastic modulus of 7.9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.7 % Show Supplier Material materials with Elongation of 2.7 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 7 GPa Show Supplier Material materials with Flexural modulus of 7 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 180 MPa Show Supplier Material materials with Flexural strength of 180 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 109 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 109 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 54 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 54 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 901 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 901 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 16 J Show Supplier Material materials with Instrumented Impact, Total Energy of 16 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 107 MPa Show Supplier Material materials with Tensile strength of 107 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2E-6 1/K | ASTM D 696 | -30°C to 30°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7E-6 1/K | ASTM D 696 | -30°C to 30°C | ||
Heat deflection temperature | 141 - 145 °C Show Supplier Material materials with Heat deflection temperature of 141 - 145 °C | ||||
Heat deflection temperature, 0.45 MPa | 145 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 145 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 141 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344533- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Individual Equiptment | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |