General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | ASTM D 792 |
Relative density | 23.0 °C | 1.35 [-] Show Supplier Material materials with Relative density of 1.35 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4.2 GPa Show Supplier Material materials with Elastic modulus of 4.2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.4 % Show Supplier Material materials with Elongation of 3.4 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 4 GPa Show Supplier Material materials with Flexural modulus of 4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 121 MPa Show Supplier Material materials with Flexural strength of 121 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 158 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 158 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 37 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 37 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 636 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 636 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 22 J Show Supplier Material materials with Instrumented Impact, Total Energy of 22 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 71 MPa Show Supplier Material materials with Tensile strength of 71 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 140 - 145 °C Show Supplier Material materials with Heat deflection temperature of 140 - 145 °C | ||
Heat deflection temperature, 0.45 MPa | 145 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 145 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344538- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |