General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.53 g/cm³ Show Supplier Material materials with Density of 1.53 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 14.5 GPa Show Supplier Material materials with Elastic modulus of 14.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.1 % Show Supplier Material materials with Elongation of 2.1 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 12 GPa Show Supplier Material materials with Flexural modulus of 12 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 315 MPa Show Supplier Material materials with Flexural strength of 315 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 13 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 55 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 55 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Tensile strength | 23.0 °C | 234 MPa Show Supplier Material materials with Tensile strength of 234 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.3E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 5.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.3E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284057- - <br> UL Recognized, 94HB Flame Class Rating: 0.8mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.14 % Show Supplier Material materials with Shrinkage of 0.14 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Circuit Protection | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |