General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.65 g/cm³ Show Supplier Material materials with Density of 1.65 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.26 % Show Supplier Material materials with Moisture absorption of 0.26 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 12.1 GPa Show Supplier Material materials with Elastic modulus of 12.1 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.7 % Show Supplier Material materials with Elongation of 1.7 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 12.3 GPa Show Supplier Material materials with Flexural modulus of 12.3 GPa | ISO 178 |
Flexural strength | 23.0 °C | 264 MPa Show Supplier Material materials with Flexural strength of 264 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 9 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 44 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 44 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 550 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 2 J Show Supplier Material materials with Instrumented Impact, at Peak of 2 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 166 MPa Show Supplier Material materials with Tensile strength of 166 MPa | ISO 527 | break |
Thermal
Property | Value |
---|---|
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101377968- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |