General
Property | Temperature | Value | Comment |
---|---|---|---|
Moisture absorption | 23.0 °C | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.25 [-] Show Supplier Material materials with Relative density of 1.25 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.6 % Show Supplier Material materials with Water absorption of 0.6 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastic modulus of 2.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4 % Show Supplier Material materials with Elongation of 4 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 88 MPa Show Supplier Material materials with Flexural strength of 88 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 294 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 294 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 294 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 294 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 53 MPa Show Supplier Material materials with Tensile strength of 53 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 99 °C Show Supplier Material materials with Heat deflection temperature of 99 °C | ||
Heat deflection temperature, 1.80 MPa | 99 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 99 °C | ASTM D 648 | 3.2mm, unannealed | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228455- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥2mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 5.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 5.00E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 17 g/10min Show Supplier Material materials with Melt mass-flow rate of 17 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |