General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.48 - 0.51 [-] Show Supplier Material materials with Coefficient of friction of 0.48 - 0.51 [-] | ||
Coefficient of friction, kinetic | 0.48 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.48 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.51 [-] Show Supplier Material materials with Coefficient of friction, static of 0.51 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.69 g/cm³ Show Supplier Material materials with Density of 1.69 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.09 % Show Supplier Material materials with Moisture absorption of 0.09 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.7 [-] Show Supplier Material materials with Relative density of 1.7 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 12.9 GPa Show Supplier Material materials with Elastic modulus of 12.9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.9 % Show Supplier Material materials with Elongation of 1.9 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 11.6 GPa Show Supplier Material materials with Flexural modulus of 11.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 192 MPa Show Supplier Material materials with Flexural strength of 192 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 13 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 138 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 138 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 42 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 42 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 647 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 647 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 17 J Show Supplier Material materials with Instrumented Impact, Total Energy of 17 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 127 MPa Show Supplier Material materials with Tensile strength of 127 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.9E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 3.9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 3.9E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Heat deflection temperature | 138 - 145 °C Show Supplier Material materials with Heat deflection temperature of 138 - 145 °C | ||||
Heat deflection temperature, 0.45 MPa | 145 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 145 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 138 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 138 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344609- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |