General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.162 g/cm³ Show Supplier Material materials with Density of 1.162 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 10 % Show Supplier Material materials with Elongation of 10 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 4 GPa Show Supplier Material materials with Flexural modulus of 4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 155 MPa Show Supplier Material materials with Flexural strength of 155 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Tensile strength | 23.0 °C | 89 MPa Show Supplier Material materials with Tensile strength of 89 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3.9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.9E-5 1/K | ASTM E 831 | -20°C to 150°C |
Vicat softening temperature | 240 °C Show Supplier Material materials with Vicat softening temperature of 240 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Electrical, Electronic Components, Enclosures, Enclosure/Housing/Cover, Exterior Trim, Forward Lighting, Fixture Bath/Shower, Fog Lamp, Lab Ware and Clinical Diagnostics, Lawn/Garden, Individual Equiptment, Recreational Vehicle, Power Boat, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Plumbing, Wireless Communications | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Rear - Zone 1 Temperature: 265 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |