General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 23.5 GPa Show Supplier Material materials with Elastic modulus of 23.5 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 1.8 % Show Supplier Material materials with Elongation of 1.8 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 25 GPa Show Supplier Material materials with Flexural modulus of 25 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 366 MPa Show Supplier Material materials with Flexural strength of 366 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 70 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 70 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 70 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 775 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 775 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 270 MPa Show Supplier Material materials with Tensile strength of 270 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 327 - 341 °C Show Supplier Material materials with Heat deflection temperature of 327 - 341 °C | |
Heat deflection temperature, 0.45 MPa | 341 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 341 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 327 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 327 °C | ASTM D 648 | 3.2mm, unannealed |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |