General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.42 g/cm³ Show Supplier Material materials with Density of 1.42 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 19.1 GPa Show Supplier Material materials with Elastic modulus of 19.1 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 0.8 % Show Supplier Material materials with Elongation of 0.8 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 16.1 GPa Show Supplier Material materials with Flexural modulus of 16.1 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 208 MPa Show Supplier Material materials with Flexural strength of 208 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 4 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 47 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 47 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 12 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 254 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 254 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 146 MPa Show Supplier Material materials with Tensile strength of 146 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 262 - 279 °C Show Supplier Material materials with Heat deflection temperature of 262 - 279 °C | |
Heat deflection temperature, 0.45 MPa | 279 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 279 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 262 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 262 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |