General
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ASTM D 638 | 50 mm/min | ||
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ISO 527 | yield | ||
Flexural modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 98 MPa Show Supplier Material materials with Flexural strength of 98 MPa | ISO 178 | ||
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 | ||
Impact strength, Charpy notched | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m² | ISO 179/2C | 23°C | ||
Impact strength, Izod notched | 23.0 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 75 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 750 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 750 J/m | ASTM D 256 | notched, 23°C | ||
Tensile strength | 23.0 °C | 68 MPa Show Supplier Material materials with Tensile strength of 68 MPa | ISO 527 | break | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 3 [-] | ASTM D 150 |
Dissipation factor, 100Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 1E-3 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2E-3 [-] | ASTM D 150 |
Volume resistivity | 23.0 °C | 2.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 2.00E+17 Ω·cm | ASTM D 257 |
Optical
Property | Value | Comment |
---|---|---|
Refractive index | 1.59 [-] Show Supplier Material materials with Refractive index of 1.59 [-] | ISO 489 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 12 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 12 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |