General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.21 [-] Show Supplier Material materials with Relative density of 1.21 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched | 23.0 °C | 694 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 694 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 694 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 694 J/m | ASTM D 256 | notched, 23°C |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 23.8 g/10min Show Supplier Material materials with Melt mass-flow rate of 23.8 g/10min | ASTM D 1238 | 300°C/1.2 kgf |
Melt volume-flow rate | 23 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 23 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |