General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.29 g/cm³ Show Supplier Material materials with Density of 1.29 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 5 % Show Supplier Material materials with Elongation of 5 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 86 MPa Show Supplier Material materials with Flexural strength of 86 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 60 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 750 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 750 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 47 MPa Show Supplier Material materials with Tensile strength of 47 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 113 °C Show Supplier Material materials with Heat deflection temperature of 113 °C | ||||
Heat deflection temperature, 1.80 MPa | 113 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 113 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat softening temperature | 128 °C Show Supplier Material materials with Vicat softening temperature of 128 °C | ASTM D 1525 | Rate A/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102180157- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥1mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant | 23.0 °C | 3.08 [-] Show Supplier Material materials with Dielectric constant of 3.08 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 1GHz | 23.0 °C | 3.06 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 3.06 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 3.08 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 3.08 [-] | SABIC method |
Dissipation factor | 23.0 °C | 6.1E-3 [-] Show Supplier Material materials with Dissipation factor of 6.1E-3 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 6.3E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6.3E-3 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 5.9E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 5.9E-3 [-] | SABIC method |
Sheet resistivity, ROA | 23.0 °C | 1.20E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.20E+16 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.20E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.20E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 25 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 25 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Wearables, Personal Computing, Enclosures, Antenna | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |