General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Density of 1.33 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1.6 % Show Supplier Material materials with Elongation of 1.6 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 11 GPa Show Supplier Material materials with Flexural modulus of 11 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 149 MPa Show Supplier Material materials with Flexural strength of 149 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 320 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 320 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 87 MPa Show Supplier Material materials with Tensile strength of 87 MPa | ASTM D 638 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283898- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101284109- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
High Volt Arc Track Rate | 23.0 °C | 0 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 0 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 4 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |