General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Density of 1.22 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Water absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Water absorption of 0.01 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 75 % Show Supplier Material materials with Elongation of 75 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 79 MPa Show Supplier Material materials with Flexural strength of 79 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 550 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 550 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 550 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 46 MPa Show Supplier Material materials with Tensile strength of 46 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 106 °C Show Supplier Material materials with Heat deflection temperature of 106 °C | ||||
Heat deflection temperature, 1.80 MPa | 106 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 106 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100974177- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.6mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.94 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.94 [-] | IEC 60250 |
Dissipation factor, 1GHz | 23.0 °C | 5.7E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 5.7E-3 [-] | IEC 60250 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 14 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 14 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage, transverse of 0.6 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Enclosures, Electronic Components, Wireless Communications, Vacuum Cleaner | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 85 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |