General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.95 g/cm³ Show Supplier Material materials with Density of 1.95 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4.1 GPa Show Supplier Material materials with Elastic modulus of 4.1 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4.7 % Show Supplier Material materials with Elongation of 4.7 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 4.4 GPa Show Supplier Material materials with Flexural modulus of 4.4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 102 MPa Show Supplier Material materials with Flexural strength of 102 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 46 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 46 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 20 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 294 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 294 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 122 °C Show Supplier Material materials with Heat deflection temperature of 122 °C | ||
Heat deflection temperature, 1.80 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284064- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=102991930- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 8 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.64 % Show Supplier Material materials with Shrinkage of 0.64 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.56 % Show Supplier Material materials with Shrinkage, transverse of 0.56 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 105°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |