General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.61 [-] Show Supplier Material materials with Relative density of 1.61 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 14.1 GPa Show Supplier Material materials with Elastic modulus of 14.1 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.2 % Show Supplier Material materials with Elongation of 2.2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 11.9 GPa Show Supplier Material materials with Flexural modulus of 11.9 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 206 MPa Show Supplier Material materials with Flexural strength of 206 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Charpy unnotched | 23.0 °C | 43 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 43 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Izod notched | 23.0 °C | 166 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 166 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 166 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 166 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 669 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 669 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 152 MPa Show Supplier Material materials with Tensile strength of 152 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 128 °C Show Supplier Material materials with Heat deflection temperature of 128 °C | ||||
Heat deflection temperature, 0.45 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 128 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102010576- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 18 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.05 % Show Supplier Material materials with Shrinkage of 0.05 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage, transverse of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Smart/ID Card, Photo/Video Camera, Wireless Communications, Document Handling, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |