General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.21 [-] Show Supplier Material materials with Relative density of 1.21 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 200 % Show Supplier Material materials with Elongation of 200 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 2 GPa Show Supplier Material materials with Flexural modulus of 2 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 80 MPa Show Supplier Material materials with Flexural strength of 80 MPa | ASTM D 790 | yield, 6.4 mm |
Impact strength, Izod notched | 23.0 °C | 700 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 700 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 700 J/m | ASTM D 256 |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 100 °C Show Supplier Material materials with Heat deflection temperature of 100 °C | ||
Heat deflection temperature, 1.80 MPa | 100 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 100 °C | ASTM D 648 | 6.4 mm, unannealed | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228454- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.20E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.20E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 19 g/10min Show Supplier Material materials with Melt mass-flow rate of 19 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 1.5-3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | SABIC method | 1.5-3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Pallet, Photo/Video Camera, Data Management, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |