Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | SABIC - Japan Method | break |
Flexural modulus | 23.0 °C | 17.5 GPa Show Supplier Material materials with Flexural modulus of 17.5 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 238 MPa Show Supplier Material materials with Flexural strength of 238 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 76 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 76 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 76 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 76 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 166 MPa Show Supplier Material materials with Tensile strength of 166 MPa | SABIC - Japan Method | yield |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | ||||
Heat deflection temperature, 0.45 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236843- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Toy | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |