General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.35 g/cm³ Show Supplier Material materials with Density of 1.35 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1.8 % Show Supplier Material materials with Elongation of 1.8 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 11.9 GPa Show Supplier Material materials with Flexural modulus of 11.9 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 177 MPa Show Supplier Material materials with Flexural strength of 177 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 25 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Tensile strength | 23.0 °C | 121 MPa Show Supplier Material materials with Tensile strength of 121 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 139 °C Show Supplier Material materials with Heat deflection temperature of 139 °C | ||
Heat deflection temperature, 1.80 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 139 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101343782- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥4.5mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.8mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.15 % Show Supplier Material materials with Shrinkage of 0.15 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |