General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | SABIC - Japan Method | break |
Flexural modulus | 23.0 °C | 6.5 GPa Show Supplier Material materials with Flexural modulus of 6.5 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 190 MPa Show Supplier Material materials with Flexural strength of 190 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 78 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 78 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 78 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 78 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 125 MPa Show Supplier Material materials with Tensile strength of 125 MPa | SABIC - Japan Method | yield |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 213 °C Show Supplier Material materials with Heat deflection temperature of 213 °C | ||
Heat deflection temperature, 0.45 MPa | 213 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 213 °C | ASTM D 648 | 3.2 mm, unannealed | |
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236987- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Amusement Machine, Additive Semiconductor Materials, Electronic Components, Enclosure/Housing/Cover, Semiconductor, Personal Computing | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |