General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Density of 1.24 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.24 % Show Supplier Material materials with Moisture absorption of 0.24 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.24 [-] Show Supplier Material materials with Relative density of 1.24 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 151 % Show Supplier Material materials with Elongation of 151 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 89 MPa Show Supplier Material materials with Flexural strength of 89 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 58 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 58 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 741 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 741 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 63 J Show Supplier Material materials with Instrumented Impact, Total Energy of 63 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 55 MPa Show Supplier Material materials with Tensile strength of 55 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.1E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.93E-3 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.93E-3 1/K | ASTM D 696 | -30°C to 30°C | ||
Heat deflection temperature | 124 - 136 °C Show Supplier Material materials with Heat deflection temperature of 124 - 136 °C | ||||
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101212682- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Energy Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |