Property | Temperature | Value | Comment |
---|---|---|---|
Compressive strength | 23.0 °C | 215 MPa Show Supplier Material materials with Compressive strength of 215 MPa | SABIC method |
Elastic modulus | 23.0 °C | 40.4 GPa Show Supplier Material materials with Elastic modulus of 40.4 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.4 % Show Supplier Material materials with Elongation of 1.4 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 33.8 GPa Show Supplier Material materials with Flexural modulus of 33.8 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 460 MPa Show Supplier Material materials with Flexural strength of 460 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 82 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 82 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 82 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 82 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 863 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 863 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Poisson's ratio | 23.0 °C | 0.5 [-] Show Supplier Material materials with Poisson's ratio of 0.5 [-] | ASTM E 132 |
Shear modulus | 23.0 °C | 5 GPa Show Supplier Material materials with Shear modulus of 5 GPa | ASTM D732 |
Shear strength | 23.0 °C | 126 MPa Show Supplier Material materials with Shear strength of 126 MPa | ASTM D732 |
Tensile strength | 23.0 °C | 321 MPa Show Supplier Material materials with Tensile strength of 321 MPa | ISO 527 | break, 5 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Aerospace | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |