Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.33 [-] Show Supplier Material materials with Relative density of 1.33 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 31 GPa Show Supplier Material materials with Elastic modulus of 31 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 1.6 % Show Supplier Material materials with Elongation of 1.6 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 24.4 GPa Show Supplier Material materials with Flexural modulus of 24.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 386 MPa Show Supplier Material materials with Flexural strength of 386 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 101 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 101 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 101 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 101 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 276 MPa Show Supplier Material materials with Tensile strength of 276 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |