LNP™ THERMOCOMP™ Compound ZX08309

Want to keep this datasheet? Save it now in your required format

Description

This material is mineral filled PPO grade with high dielectric constant and low loss tangent

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.66 g/cm³

Show Supplier Material materials with Density of 1.66 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Impact strength, Izod notched

23.0 °C

60 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 60 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

60 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 60 J/m

ASTM D 256 | notched, 23°C

Thermal

PropertyValueComment

Heat deflection temperature

122 - 134 °C

Show Supplier Material materials with Heat deflection temperature of 122 - 134 °C

Heat deflection temperature, 0.45 MPa

134 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 134 °C

ASTM D 648 | 3.2 mm, unannealed

Heat deflection temperature, 1.80 MPa

122 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C

ASTM D 648 | 3.2mm, unannealed

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1GHz

23.0 °C

4.4 [-]

Show Supplier Material materials with Dielectric constant, 1GHz of 4.4 [-]

ASTM ES 7-83 | 1.1 GHz

Dissipation factor, 1GHz

23.0 °C

2E-3 [-]

Show Supplier Material materials with Dissipation factor, 1GHz of 2E-3 [-]

ASTM ES 7-83 | 1.1 GHz

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

11 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 11 cm³/10min

ISO 1133 | MVR at 300°C/5.0 kg

Shrinkage

23.0 °C

0.7 %

Show Supplier Material materials with Shrinkage of 0.7 %

ASTM D 955 | 24 hrs

Shrinkage, transverse

23.0 °C

0.65 %

Show Supplier Material materials with Shrinkage, transverse of 0.65 %

ASTM D 955 | 24 hrs

Technological properties

Property
Application areas

Wireless Communications, Wiring Devices, Cooking Range

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 105°C
Drying Time: 3 to 5.0hrs
Melt Temperature: 295 to 305.0°C
Nozzle Temperature: 290 to 295.0°C
Front - Zone 3 Temperature: 300 to 305.0°C
Middle - Zone 2 Temperature: 290 to 295.0°C
Rear - Zone 1 Temperature: 280 to 285.0°C
Mold Temperature: 90°C
Back Pressure: 9MPa
Screw Speed: 100rpm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.