General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.28 g/cm³ Show Supplier Material materials with Density of 1.28 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.89 % Show Supplier Material materials with Moisture absorption of 0.89 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.28 [-] Show Supplier Material materials with Relative density of 1.28 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 0.1 GPa Show Supplier Material materials with Elastic modulus of 0.1 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 388 % Show Supplier Material materials with Elongation of 388 % | ASTM D 638 | yld, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 0.1 GPa Show Supplier Material materials with Flexural modulus of 0.1 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Instrumented Impact, Total Energy | 23.0 °C | 39 J Show Supplier Material materials with Instrumented Impact, Total Energy of 39 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 19 MPa Show Supplier Material materials with Tensile strength of 19 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 23 °C Show Supplier Material materials with Heat deflection temperature of 23 °C | |
Heat deflection temperature, 0.45 MPa | 23 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 23 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm |
Heat deflection temperature, 1.80 MPa | 23 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 23 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 100000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 100000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |