General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 50 - 100 % Show Supplier Material materials with Elongation of 50 - 100 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 2.7 GPa Show Supplier Material materials with Flexural modulus of 2.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 106 MPa Show Supplier Material materials with Flexural strength of 106 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 70.3 MPa Show Supplier Material materials with Tensile strength of 70.3 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.6E-5 1/K | ASTM D 696 | -30°C to 30°C |
Heat deflection temperature | 174 °C Show Supplier Material materials with Heat deflection temperature of 174 °C | ||
Heat deflection temperature, 1.80 MPa | 174 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 174 °C | ASTM D 648 | 3.2mm, unannealed |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1MHz | 23.0 °C | 3.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.02 [-] | ASTM D 150 | |
Dissipation factor, 1kHz | 23.0 °C | 3.04 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 3.04 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 3.03 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3.03 [-] | ASTM D 150 | 50/60 Hz |
Volume resistivity | 23.0 °C | 5.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 5.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 17 g/10min Show Supplier Material materials with Melt mass-flow rate of 17 g/10min | ASTM D 1238 | 330°C/2.16 kgf | |
Shrinkage | 23.0 °C | 0.7 % Show Supplier Material materials with Shrinkage of 0.7 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Others, Surgical Tray, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 135 to 163.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |