General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 4.1 GPa Show Supplier Material materials with Flexural modulus of 4.1 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 124 MPa Show Supplier Material materials with Flexural strength of 124 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 3 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 15 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Tensile strength | 23.0 °C | 74 MPa Show Supplier Material materials with Tensile strength of 74 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.1E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Heat deflection temperature | 111 °C Show Supplier Material materials with Heat deflection temperature of 111 °C | ||
Heat deflection temperature, 1.80 MPa | 111 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 111 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt volume-flow rate | 27 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 27 cm³/10min | ISO 1133 | MVR at 340°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |