General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Density of 1.43 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 23.9 GPa Show Supplier Material materials with Elastic modulus of 23.9 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 1.2 % Show Supplier Material materials with Elongation of 1.2 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 21.2 GPa Show Supplier Material materials with Flexural modulus of 21.2 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 282 MPa Show Supplier Material materials with Flexural strength of 282 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 74 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 74 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 186 MPa Show Supplier Material materials with Tensile strength of 186 MPa | ASTM D 638 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 108 °C Show Supplier Material materials with Heat deflection temperature of 108 °C | ||
Heat deflection temperature, 1.80 MPa | 108 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 108 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |
Flammability | UL Recognized, 94V-0 Flame Class Rating: 1mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093470- - |
Technological properties
Property | ||
---|---|---|
Application areas | Conveyor | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |