General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 7.1 GPa Show Supplier Material materials with Elastic modulus of 7.1 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.2 % Show Supplier Material materials with Elongation of 2.2 % | ISO 527 | break, 5 mm/min |
Flexural strength | 23.0 °C | 140 MPa Show Supplier Material materials with Flexural strength of 140 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 66 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 66 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 386 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 386 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 93 MPa Show Supplier Material materials with Tensile strength of 93 MPa | ISO 527 | break, 5 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, ATM/Ticket Machine | |
Availability | Asia,Americas | |
Processing methods | Melt Temperature: 305 to 325.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |