General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 47 % Show Supplier Material materials with Limiting oxygen index of 47 % | |
Moisture absorption | 23.0 °C | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.27 [-] Show Supplier Material materials with Relative density of 1.27 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 1.25 % Show Supplier Material materials with Water absorption of 1.25 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 3.3 GPa Show Supplier Material materials with Flexural modulus of 3.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 160 MPa Show Supplier Material materials with Flexural strength of 160 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1335 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1335 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | ||||
Heat deflection temperature, 1.80 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 215 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Vicat softening temperature | 215 °C Show Supplier Material materials with Vicat softening temperature of 215 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100044765- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 0.7- ASTM E 662 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Dielectric strength | 23.0 °C | 27.9 kV/mm Show Supplier Material materials with Dielectric strength of 27.9 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Dissipation factor | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Dissipation factor of 2.5E-3 [-] | ASTM D 150 | 2450 MHz |
Dissipation factor, 1kHz | 23.0 °C | 1.3E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 1.3E-3 [-] | ASTM D 150 |
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 9 g/10min Show Supplier Material materials with Melt mass-flow rate of 9 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Melt volume-flow rate | 13 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 13 cm³/10min | ISO 1133 | MVR at 220°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Delivery, Lab Ware and Clinical Diagnostics, Electronic Components, Animal Testing, Surgical Tray, Pharmaceutical Manufacturing, Pharmaceutical Packaging & Drug Delivery, Surgical Devices, Respiratory, Renal and Blood Handling, Oil/Gas, Medical Facility Infrastructure, Monitoring and Imaging, LED Lighting, Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |