Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.19 [-] Show Supplier Material materials with Relative density of 1.19 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 7.7 % Show Supplier Material materials with Elongation of 7.7 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 5.6 GPa Show Supplier Material materials with Flexural modulus of 5.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 129 MPa Show Supplier Material materials with Flexural strength of 129 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 165 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 165 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 165 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 165 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 827 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 827 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 19 J Show Supplier Material materials with Instrumented Impact, Total Energy of 19 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 79 MPa Show Supplier Material materials with Tensile strength of 79 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.44E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.44E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7.74E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.74E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 133 - 155 °C Show Supplier Material materials with Heat deflection temperature of 133 - 155 °C | ||||
Heat deflection temperature, 0.45 MPa | 155 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 155 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ASTM D 648 | 3.2mm, unannealed | |||
Vicat softening temperature | 162 °C Show Supplier Material materials with Vicat softening temperature of 162 °C | ASTM D 1525 | Rate B/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221227- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 2.6 g/10min Show Supplier Material materials with Melt mass-flow rate of 2.6 g/10min | ASTM D 1238 | 260°C/5.0 kgf | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.25 % Show Supplier Material materials with Shrinkage, transverse of 0.25 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe/Fitting | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 65 to 75.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |