Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 7.7 % Show Supplier Material materials with Elongation of 7.7 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 5.6 GPa Show Supplier Material materials with Flexural modulus of 5.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 129 MPa Show Supplier Material materials with Flexural strength of 129 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 165 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 165 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 79 MPa Show Supplier Material materials with Tensile strength of 79 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.44E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.44E-5 1/K | ASTM E 831 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 7.74E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.74E-5 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature | 133 - 155 °C Show Supplier Material materials with Heat deflection temperature of 133 - 155 °C | ||
Heat deflection temperature, 0.45 MPa | 155 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 155 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ASTM D 648 | 3.2mm, unannealed | |
Vicat softening temperature | 162 °C Show Supplier Material materials with Vicat softening temperature of 162 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Power Boat, Weapon, Water Treatment/Filtration, Vacuum Cleaner, Furnace/Heater, Hot Water System, Enclosures, Electronic Components, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |