General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.9 GPa Show Supplier Material materials with Elastic modulus of 3.9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 3.7 GPa Show Supplier Material materials with Flexural modulus of 3.7 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 115 MPa Show Supplier Material materials with Flexural strength of 115 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 118 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 118 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, -30°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 449 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 449 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 21 J Show Supplier Material materials with Instrumented Impact, Total Energy of 21 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 64 MPa Show Supplier Material materials with Tensile strength of 64 MPa | ISO 527 | break |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 129 - 132 °C Show Supplier Material materials with Heat deflection temperature of 129 - 132 °C | ||||
Heat deflection temperature, 0.45 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 132 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 129 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 90 °C Show Supplier Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 90 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 90 °C | UL 746B | |||
Vicat softening temperature | 140 °C Show Supplier Material materials with Vicat softening temperature of 140 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228544- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237019- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 16.6 g/10min Show Supplier Material materials with Melt mass-flow rate of 16.6 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Melt volume-flow rate | 4 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 4 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Water System, Plumbing, Water Treatment/Filtration | |
Availability | Asia,Americas | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |