General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.06 g/cm³ Show Supplier Material materials with Density of 1.06 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 22 % Show Supplier Material materials with Limiting oxygen index of 22 % | |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.06 [-] Show Supplier Material materials with Relative density of 1.06 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.23 % Show Supplier Material materials with Water absorption of 0.23 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.7 GPa Show Supplier Material materials with Elastic modulus of 2.7 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 95 MPa Show Supplier Material materials with Flexural strength of 95 MPa | ISO 178 | yield, 2 mm/min |
Gardner Impact | 23.0 °C | 25 J Show Supplier Material materials with Gardner Impact of 25 J | ASTM D 3029 | -30°C |
Hardness, Rockwell R | 23.0 °C | 119 [-] Show Supplier Material materials with Hardness, Rockwell R of 119 [-] | ASTM D 785 |
Impact strength, Charpy notched | 23.0 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 17 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Impact strength, Izod notched | 23.0 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 17 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 213 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 213 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 48 J Show Supplier Material materials with Instrumented Impact, Total Energy of 48 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 51 MPa Show Supplier Material materials with Tensile strength of 51 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9.18E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9.18E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 9.54E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9.54E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 120 - 131 °C Show Supplier Material materials with Heat deflection temperature of 120 - 131 °C | ||||
Heat deflection temperature, 0.45 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 131 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat softening temperature | 140 °C Show Supplier Material materials with Vicat softening temperature of 140 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228539- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237006- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 3 V Show Supplier Material materials with Comparative tracking index of 3 V | UL 746A | (UL) {PLC} |
Dielectric constant, 60Hz | 23.0 °C | 2.65 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.65 [-] | ASTM D 150 | 50/60 Hz |
Dielectric strength | 23.0 °C | 21.6 kV/mm Show Supplier Material materials with Dielectric strength of 21.6 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 50Hz | 23.0 °C | 4E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-4 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 9.2 g/10min Show Supplier Material materials with Melt mass-flow rate of 9.2 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Melt volume-flow rate | 9 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover, Electronic Components, Fused Deposition Modeling (FDM), Water Treatment/Filtration, Pump, Medical Device, Meter Water | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 105 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |