General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.13 g/cm³ Show Supplier Material materials with Density of 1.13 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ASTM D 570 | (50% RH, Equilibrium) |
Water absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Water absorption of 0.2 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4.9 GPa Show Supplier Material materials with Elastic modulus of 4.9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.7 % Show Supplier Material materials with Elongation of 2.7 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 4.9 GPa Show Supplier Material materials with Flexural modulus of 4.9 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 135 MPa Show Supplier Material materials with Flexural strength of 135 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Charpy unnotched | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 14 kJ/m² | ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C |
Impact strength, Izod notched | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 4 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 35 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 35 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 13 kJ/m² | ISO 180/1U | unnotched 80*10*4, -30°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 230 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 230 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 94 MPa Show Supplier Material materials with Tensile strength of 94 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature | 126 - 135 °C Show Supplier Material materials with Heat deflection temperature of 126 - 135 °C | ||
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Vicat softening temperature | 140 °C Show Supplier Material materials with Vicat softening temperature of 140 °C | ISO 306 | Rate B/120 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 32 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 32 cm³/10min | ISO 1133 | MVR at 280°C/10.0 kg | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Water Treatment/Filtration, Meter Water, Pump, Energy Management, Hot Water System, Fixture Bath/Shower, Coffee Maker/Espresso Machine | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |