General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.22 [-] Show Supplier Material materials with Relative density of 1.22 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 4 % Show Supplier Material materials with Elongation of 4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 4.6 GPa Show Supplier Material materials with Flexural modulus of 4.6 GPa | ASTM D 790 | 6.4 mm |
Flexural strength | 23.0 °C | 102 MPa Show Supplier Material materials with Flexural strength of 102 MPa | ASTM D 790 | yield, 6.4 mm |
Impact strength, Izod notched | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 35 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 35 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 35 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.2E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 4.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 103 °C Show Supplier Material materials with Heat deflection temperature of 103 °C | ||||
Heat deflection temperature, 1.80 MPa | 103 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 103 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Flammability | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100140832- - |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | ASTM D 1238 | 300°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Asia | |
Processing methods | Rear - Zone 1 Temperature: 220 to 270.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |