General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative density of 1.2 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 4 % Show Supplier Material materials with Elongation of 4 % | ASTM D 638 | yld, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 89 MPa Show Supplier Material materials with Flexural strength of 89 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 550 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 550 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 550 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 65 J Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 63 MPa Show Supplier Material materials with Tensile strength of 63 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 78 °C Show Supplier Material materials with Heat deflection temperature of 78 °C | |
Heat deflection temperature, 1.80 MPa | 78 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 78 °C | ASTM D 648 | 3.2mm, unannealed |
Vicat softening temperature | 102 °C Show Supplier Material materials with Vicat softening temperature of 102 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 26 g/10min Show Supplier Material materials with Melt mass-flow rate of 26 g/10min | ASTM D 1238 | 266°C/5.0 kgf | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Power Manangement, Safety Glasses, Renal and Blood Handling, Medical Facility Infrastructure, Monitoring and Imaging, Medical Device, Navigation Unit, Personal Computing, Watch/Jewelry, Wearables, Wireless Communications, Vending Machine, Displays, Audio, Enclosure/Housing/Cover, Enclosures, Electronic Components, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |