General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Density of 1.3 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.3 [-] Show Supplier Material materials with Relative density of 1.3 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 1.25 % Show Supplier Material materials with Water absorption of 1.25 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 25 % Show Supplier Material materials with Elongation of 25 % | ISO 527 | break, 5 mm/min | ||
Flexural modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Flexural modulus of 3.2 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 130 MPa Show Supplier Material materials with Flexural strength of 130 MPa | ISO 178 | yield, 2 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 127 MPa Show Supplier Material materials with Hardness, Ball Indentation of 127 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Charpy notched | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm | ||
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2100 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2100 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 40 J Show Supplier Material materials with Instrumented Impact, Total Energy of 40 J | ASTM D 3763 | 23°C | ||
Taber Abrasion | 23.0 °C | 15 mg/1000cy Show Supplier Material materials with Taber Abrasion of 15 mg/1000cy | SABIC method | CS-17, 1 kg | ||
Tensile strength | 23.0 °C | 90 MPa Show Supplier Material materials with Tensile strength of 90 MPa | ISO 527 | yield, 5 mm/min | ||
Impact strength, Charpy unnotched | ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C | ||||
Impact strength, Izod unnotched | ISO 180/1U | unnotched 80*10*4, -30°C |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Passes | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Heat deflection temperature | 185 - 200 °C Show Supplier Material materials with Heat deflection temperature of 185 - 200 °C | ||||
Heat deflection temperature, 0.45 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 185 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 185 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 0.26 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.26 W/(m·K) | ISO 8302 | ||
Vicat softening temperature | 200 °C Show Supplier Material materials with Vicat softening temperature of 200 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221074- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 2 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 2.4 g/10min Show Supplier Material materials with Melt mass-flow rate of 2.4 g/10min | ASTM D 1238 | 295°C/6.6 kgf | |
Melt volume-flow rate | 15 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 15 cm³/10min | ISO 1133 | MVR at 340°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | SABIC method | on tensile bar |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Interior Rail Components, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 135°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |