General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 8 - 10 % Show Supplier Material materials with Elongation of 8 - 10 % | SABIC - Japan Method | break |
Flexural modulus | 23.0 °C | 7.4 GPa Show Supplier Material materials with Flexural modulus of 7.4 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 159 MPa Show Supplier Material materials with Flexural strength of 159 MPa | ASTM D 790 |
Hardness, Rockwell R | 23.0 °C | 121 [-] Show Supplier Material materials with Hardness, Rockwell R of 121 [-] | ASTM D 785 |
Impact strength, Izod notched | 23.0 °C | 127 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 127 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 127 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 127 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 117 MPa Show Supplier Material materials with Tensile strength of 117 MPa | SABIC - Japan Method | yield |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2E-5 - 4.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2E-5 - 4.3E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature | 140 °C Show Supplier Material materials with Heat deflection temperature of 140 °C | ||||
Heat deflection temperature, 1.80 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Flammability | UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.93 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.93 [-] | ASTM D 150 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 8.3 g/10min Show Supplier Material materials with Melt mass-flow rate of 8.3 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Hot Water System, Enclosures, Electronic Components, Dishwasher, Meter Water, Pump, Plumbing, Photo/Video Camera | |
Availability | Asia | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |